brand: | Baiya | payment terms: | L/C, D/A, D/P, T/T, Western Union, MoneyGram, Paypal |
product name: | China high quality soft TPR shrimp bait material | Origin: | Jiangsu, China |
color: | natural or custom | density: | 1.15±0.05 |
appearance: | Plastic particles | Supply capacity: | 5000 tons per year Chinese high quality soft TPR material for shrimp bait |
delivery time: | 7-15 days | Certificate: | /EN71/ASTM |
Material: | TPR material | model: | JL007 |
hardness: | 0-100A | style: | Raw material flame retardant TPR |
tensile strength: | ≥5 |
China high quality soft TPR shrimp bait material
Product Description
commodity | TPE30C | Quality inspection date | 2018/12/13 | |||
No. | thing | unit | standard | Determine the scope | Test results | Test Methods |
1 | appearance | visual test | natural color | natural color | ||
2 | hardness | Shore A | ASTM-D2240 | 0~100 | 30℃ | Indoor temperature °C |
3 | density | SP.Gr | ASTM-792 | 1.15±0.05 | 1.2 | |
4 | solution flow index | g/10min | ASTM-D1238 | 5~20 | 13 | 190℃, 2.16kg |
5 | tensile strength | MPa | ASTM-D412 | ≥5 | 7.8 | Indoor temperature 500mm/min |
6 | elongation | % | ASTM-D412 | ≥500 | 550 | |
7 | tear strength | kN/m | ASTM-D624 | ≥20 | twenty three | |
manufacturing process | ||||||
barrel temperature | Range ℃ | Typical value °C | ||||
Front section | 150-190 | 170 | ||||
middleware | 150-210 | 180 | ||||
rear end | 150-210 | 180 | ||||
Orifice/die | 160-200 | 180 | ||||
Processing temperature upper limit ℃ | 220 | |||||
drying time | Generally, drying is not required. If the storage environment is humid or the product surface requirements are high, it can be dried in a hot air oven for 2-4 hours | |||||
1. The above data are for reference only. The above data can be adjusted according to different models, molds and product requirements. 2. The residence time of the material in the barrel should not be too long, please clean the machine with PE before stopping. | ||||||
Materials can be developed and produced according to customer requirements |